Injection moulding tolerances explained
A tolerance is the permitted variation around a nominal dimension. Moulded plastic parts vary more than machined metal parts because of shrinkage, material, wall thickness, moisture and tool wear, so standards such as ISO 20457 give a plastics-specific framework for what is realistic to specify.
A tolerance in injection moulding is the range of variation a drawing accepts around a nominal dimension. A feature drawn at 20 mm with a stated tolerance passes if the measured value sits inside the limits and fails if it does not. Tolerances also apply to form and position, such as flatness or where a hole sits relative to a datum, and ISO 20457 covers both geometrical and dimensional tolerances for plastic moulded parts.
Why do injection moulded plastic parts vary in size?
Plastic moulded parts show significantly greater variation in dimensions, form and location than metal parts because of cooling shrinkage, resin behaviour, part geometry, moisture uptake and mould wear. Tolerance approaches developed for metals cannot generally be applied directly to plastics.
Shrinkage. Thermoplastics change volume as they cool because of their compressibility and thermal expansion. The mould builder has to predict the difference between the cavity dimensions and the dimensions of the finished part. Warpage is separate from shrinkage: the shape distorts while the volume stays the same.
Material. Semicrystalline plastics are more susceptible to shrinkage than amorphous ones, and additives such as glass fibres or pigments can change how much a part shrinks. Semicrystalline grades such as polypropylene and polyamide react strongly to process temperatures, and fibre-filled plastics usually shrink unevenly in different directions depending on local fibre orientation.
Wall thickness, geometry and gate. Shrinkage depends on more than the resin alone. Part geometry, wall thickness, gate position and size, and mould and melt temperatures all affect the final size. Keeping wall thickness as thin and as uniform as possible, with gradual transitions where changes are unavoidable, helps limit uneven shrinkage and warpage.
Moisture. Freshly moulded nylon parts start absorbing moisture from the air as soon as they are ejected, which increases part dimensions. The time to reach equilibrium depends on wall thickness, moisture content and temperature, with PA66 taking up about 2.5 percent water at 50 percent relative humidity.
Tool wear. Cavity wear occurs mainly through abrasion, erosion and corrosion and can reduce the quality of moulded parts over a tool's life. Glass-reinforced polyamide in particular wears moulds significantly.
How do ISO 20457 and DIN 16742 set plastic moulding tolerances?
ISO 20457 is the current international standard for plastic moulded part tolerances and acceptance conditions, while DIN 16742 is the earlier 2013 German standard on the same subject, which succeeded DIN 16901 and is now withdrawn.
ISO 20457 provides a plastics-specific framework made up of general tolerances, direct tolerances, limits of technical manufacturability and acceptance conditions, tying achievable limits to manufacturing effort and the way plastics behave. Its second edition was published in August 2026 and replaces the 2018 edition. The standard applies to non-porous parts made from thermoplastics, thermoplastic elastomers and thermosets by injection moulding and several other processes, while surface imperfections such as sink marks, flow structures, roughness and joint lines sit outside its scope.
Is 0.01 a tight tolerance for injection moulding?
Whether 0.01 is a tight tolerance in injection moulding depends on the unit of measurement, the size of the feature and the material being moulded. One inch is exactly 25.4 mm, so 0.01 inch equals 0.254 mm and a 0.01 mm limit is 25.4 times tighter. The same numerical limit is a small fraction of a 100 mm length and a large fraction of a 2 mm detail. Because shrinkage, moisture and wear all move the finished size of a plastic part, and ISO 20457 ties achievable limits to manufacturing effort, state the unit clearly on the drawing and check with the moulder what can be held for your material and feature.
How should you specify critical tolerances on an injection moulded part?
Specify tight limits only on features that control fit or function, such as mating faces, snap fits and screw bosses, and leave other dimensions to a general tolerance note. ISO 20457 is designed to help specify functionally necessary tolerances, and because tighter limits demand greater manufacturing effort, every tight callout needs a clear functional reason.
Choose the material grade and name your datums before locking in tolerances, since shrinkage changes with the resin. Designing uniform wall thickness reduces uneven shrinkage and warpage, which helps hold every tolerance on the part.
State the measuring condition and agree acceptance conditions on the drawing so both sides measure parts the same way at the same stage. For moisture-absorbing plastics such as nylon, specify whether parts are checked as moulded or after conditioning. Shrinkage data under ISO 294-4 is quoted 24 hours after demoulding, which shows how much timing changes the measured dimension.
What injection moulding tolerances can Lianto Plastics hold?
Achievable tolerances depend on the part, material and tool, so Lianto Plastics confirms them during the engineering review before quoting rather than publishing one fixed figure for every part. During production, we inspect parts every two hours, keep a sealed approved sample on file, supply a measurement report with the first samples, and adjust small changes after first samples at no charge.
Read more about our injection moulding process, call us on 1300 214 070, or send your drawing to get a quote with an engineering review and fixed quotation.
Questions
What is the difference between ISO 20457 and DIN 16742?
Both set out tolerances and acceptance conditions for plastic moulded parts. DIN 16742 is the 2013 German standard, which DIN Media now lists as withdrawn. ISO 20457 is the international standard on the same subject, and its second edition was published in August 2026.
Why can the same moulded part measure differently on different days?
Plastics keep changing size after moulding. Shrinkage continues as the part cools, and moisture-absorbing materials such as nylon grow as they take up water from the air. Measuring conditions and timing should be agreed so results can be compared.
Should every dimension on a moulded part have a tolerance?
No. Tolerance the dimensions that decide fit or function, such as mating features, and leave the rest to a general tolerance. Tighter tolerances need more manufacturing effort, so each one should be there for a reason.
Is 0.01 a tight tolerance?
It depends on the unit and the feature. 0.01 mm is one hundredth of a millimetre, while 0.01 inch is 0.254 mm, which is 25.4 times larger. Whether either is tight depends on the feature size, the material and the process, so agree the unit and check what is achievable for your part.
What tolerance can Lianto hold?
It depends on the part, the material and the tool. Achievable tolerances for a part are confirmed in the engineering review before the quotation, once the drawing and material are known.
Sources
ISO 20457:2026 Plastics moulded parts, Tolerances and acceptance conditions, International Organization for Standardization
DIN 16742:2013-10 Plastics moulded parts, Tolerances and acceptance conditions, DIN Media
The fundamentals of shrinkage in thermoplastics, Covestro
The Dimensional Stability of Moulded Parts: A Review of the Technology Base, National Physical Laboratory
MOCOM Guideline Shrinkage, MOCOM Compounds
DuPont Zytel and Minlon nylon resins, processing guide, DuPont
Wall thickness, Envalior
Mechanism-based wear models for plastic injection moulds, Wear (Elsevier)
SI Units, Length (definition of the inch as exactly 25.4 mm), National Institute of Standards and Technology (NIST)